Title: Use of High-Range Water-Reducing Admixtures (Superplastisizers) In Residential concrete

Author(s): Michael zummo and Robert L. Henry

Publication: Concrete International

Volume: 4

Issue: 2

Appears on pages(s): 31-35

Keywords: admixtures; compressive strength; concretes; economics; mix proportioning; plasticizers; quality control; residential buildings; slump tests; water-reducing agents

DOI:

Date: 2/1/1982

Abstract:
A high-range water-reducing admixture was used in a field environment on an experimental basis by a large home builder in the Dallas-Fort Worth, Texas, area. The admixture was added to the standard concrete mixture and the normal field crews were used for placement. The effect of the admixture on slump, compressive strength, flexural strength, air entrainment, unit weight, integrity of the finished house slab, and labor performance was evaluated. Increased compressive strength, labor savings in placement times, and improved smoothness of the house slab were realized when the admixture was used.




  