Title: Crack Repair Of Precast Concrete Panels

Author(s): Brian J. Pashina

Publication: Concrete International

Volume: 8

Issue: 8

Appears on pages(s): 22-26

Keywords:

DOI:

Date: 8/1/1986

Abstract:
Cracks occur in concrete structures due to a variety of causes. The successful repair of this cracking involves: documenting the location and severity of all cracks present, identifying the cause, judging potential for crack propagation, selecting repair materials and methods, and finally, insuring good workmanship during repair. This article presents a case history of extensive cracking which was repaired using fiber reinforced mortar.