Construction Equipment For Cable-Stayed Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction Equipment For Cable-Stayed Bridges

Author(s): Boris Levintov

Publication: Concrete International

Volume: 17

Issue: 11

Appears on pages(s): 24-29

Keywords:

DOI:

Date: 11/1/1995

Abstract:
Apart from the spans of the largest suspension bridges, cable-stayed spans are among the longest in the world. Long spans, which create optimal conditions for vessel volume, navigation, and safety, can be achieved in cable-stayed construction at a fraction of the cost it takes to build a suspension span of comparable length.