Title: Some Concretes Need 7 Days Initial Curing

Author(s): M. N. Haque

Publication: Concrete International

Volume: 12

Issue: 2

Appears on pages(s): 42-46

Keywords:

DOI:

Date: 2/1/1990

Abstract:
Proper curing is essential for strength development and durability of concrete. Most codes of practice recommend sufficient curing to achieve a maturity equivalent to seven days moist curing, especially when the exposure conditions are likely to be severe.