Solidifying and Stabilizing Waste AT A Hazardous Landfill

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Solidifying and Stabilizing Waste AT A Hazardous Landfill

Author(s): S. B. Sehgal, Albin Gronowicz

Publication: Concrete International

Volume: 12

Issue: 7

Appears on pages(s): 41-44

Keywords:

DOI:

Date: 7/1/1990

Abstract:
In the early 1960s, approximately 360 drums containing the solid residue from a solution used to case harden carbon steel were buried in a landfill in a man-made excavation in Bowling Green, Kentucky.