Geopolymeric concretes For Environmental Protection

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Geopolymeric concretes For Environmental Protection

Author(s): Joseph Davidovits, Douglas C. Comrie, John H. Paterson, Douglas J. Ritcey

Publication: Concrete International

Volume: 12

Issue: 7

Appears on pages(s): 30-40

Keywords:

DOI:

Date: 7/1/1990

Abstract:
When nuclear plants began to be constructed on an international scale, industry planners assumed that by the time the reactors reached the end of their service lives (25 to 30 years) the technology would exist to render them environmentally safe by disassembly or entombment. The service lives of a number of these reactors are almost spent, but there is still considerable debate about the selection of a suit-able entombment technology.