Title: Sound Uses Of CLSMs In The Environment

Author(s): Ronald L. Larsen

Publication: Concrete International

Volume: 12

Issue: 7

Appears on pages(s): 26-29

Keywords:

DOI:

Date: 7/1/1990

Abstract:
Controlled low strength materials (CLSMs) have found acceptance for such environment-enhancing applications as protecting groundwater re-sources, minimizing damage from moving water, and alleviating problems caused by moving water. CLSMs are defined by ACI Coin¬mittee 229 as fill materials that reach 1200 psi (8274 kPa) uncon¬fined compressive strength or less.