Title: Filling Abandoned Underground Facilities With CLSM Fly Ash Slurry

Author(s): Tarun R. Naik, Bruce w. Ramme, Henry J. Kolbeck

Publication: Concrete International

Volume: 12

Issue: 7

Appears on pages(s): 19-25

Keywords:

DOI:

Date: 7/1/1990

Abstract:
The Wisconsin Electric Power Company (WE) is well along in developing a solution to the age-old problem of how to have one's cake and eat it, too: they're creating fly ash, but also using it. Working together with the University of Wisconsin-Milwaukee Center for By-Products Utilization, WE is identifying mix proportions for flowable fly ash slurry that can be used as backfill for excavation projects and as fill for abandoned underground facilities.