Title: Polymer Concrete Bridge Overlays

Author(s): Jorge Cremaschi

Publication: Concrete International

Volume: 8

Issue: 5

Appears on pages(s): 58-60

Keywords:

DOI:

Date: 5/1/1986

Abstract:
The serious deterioration of concrete roads and bridges has created a need for a practical alternative to tearing up and replacing existing bridge decks. This paper discusses the use of polymer concrete bridge overlays as a faster, less expensive alternative that protects bridge decks while offering good wear resistance and skid resistance.