Title: Why Steel Reinforcement Is Needed In Concrete Slabs

Author(s): Roy H. Reiterman

Publication: Concrete International

Volume: 18

Issue: 12

Appears on pages(s): 75-76

Keywords:

DOI:

Date: 12/1/1996

Abstract:
People are being misinformed about steel reinforcement in concrete structures. Over the last five years or more, there has been a considerable amount of advertising in the varioius concrete industry trade magazines alluding to the placing of concrete without steel reinforcement.