Drying Shrinkage Behavior Of Recycled Aggregate Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Drying Shrinkage Behavior Of Recycled Aggregate Concrete

Author(s): Mostafa Tavakoli, Parviz Soroushian

Publication: Concrete International

Volume: 18

Issue: 11

Appears on pages(s): 58-61

Keywords:

DOI:

Date: 11/1/1996

Abstract:
Recycling of concrete demolition debris obtained from reconstruction projects of structures and highways has been considered for many years. Recycling demolished concrete as aggregate helps to overcome environmental and economic problems of obtaining quality aggregate from natural sources and to facilitate concrete disposal. The studies performed by researchers on the qualities of concrete made using recycled aggregate have been reviewed in the literature.