Title: An Analysis Of concrete Framed Structures During The Construction Process

Author(s): Juan J. Moragues, Joaquin Catala, Eugenio Pelicer

Publication: Concrete International

Volume: 18

Issue: 11

Appears on pages(s): 44-48

Keywords:

DOI:

Date: 11/1/1996

Abstract:
The construction of slabs in concrete framed structures often employs shoring and formwork such that the weight of the newly cast slab plus the working load are transferred to one or more previously placed slabs.