Title: Thin, Long-Span Slabs In China

Author(s): Ding Dajun

Publication: Concrete International

Volume: 18

Issue: 8

Appears on pages(s): 35-38

Keywords:

DOI:

Date: 8/1/1996

Abstract:
In te past 30 years, China has seen the constructionof new types of precast, long-span, thin-wall concrete roof and floor slabs. This construction technology has provided economic benefits and promoted development in concrete structures.