Title: Ancient Structural Concrete In Mesoamerica

Author(s): Raymundo Rivera-Villarreal, Stefan Krayer

Publication: Concrete International

Volume: 18

Issue: 6

Appears on pages(s): 67-70

Keywords:

DOI:

Date: 6/1/1996

Abstract:
Archeological studies date the origins of the earliest inhabitants of Mesoamerica at somewhere between 30,000 and 22,000 B.C. Starting about 1000 B.C., Mesoamerican primitive societies developed an autonomous culture.