Title: Concrete Firsts

Author(s): Bryant Mather

Publication: Concrete International

Volume: 18

Issue: 6

Appears on pages(s): 43

Keywords:

DOI:

Date: 6/1/1996

Abstract:
Most of the new inventions and innovations that have led to major improvements in concrete technology turn out, on examination of the history of concrete, not to be new. What often is new is that somebody or some organization found out how to apply the invention or the innovation and its potential got a chance to be realized.