Title: A Reinforcing Steel-Free Concrete Deck Slab For the Salmon River Bridge

Author(s): John P. Newhook

Publication: Concrete International

Volume: 18

Issue: 6

Appears on pages(s): 30-34

Keywords:

DOI:

Date: 6/1/1996

Abstract:
The first known fiber reinforced concrete (FRC) bridge deck slab without any internal steel reinforcement was constructed on the Trans Canada Highway 104 and opened to traffic on December 5, 1995. A companion bridge deck with conventional steel reinforcement design was also constructed.