Design Durable Industrial Floor Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design Durable Industrial Floor Slabs

Author(s): Robert Fitzpatrick

Publication: Concrete International

Volume: 18

Issue: 1

Appears on pages(s): 38-39

Keywords:

DOI:

Date: 1/1/1996

Abstract:
Concrete floor slabs on grade are inherently problematic. This article presents three of the common causes of problems with concrete floor slabs on grade and some "state of the art" innovations in floor slab design and construction that can reduce the occurrence of these problems.