Title: Stamped Concrete is the Real Thing

Author(s): William D. Palmer

Publication: Concrete International

Volume: 7

Issue: 11

Appears on pages(s): 33-38

Keywords: colored concrete; concrete finishing (fresh concrete); stamping; tools.

DOI:

Date: 11/1/1985

Abstract:
Colored and imprinted concrete can look almost identical to brick, slate, or stone. This article examines the techniques used to create this effect and the people involved in this growing industry.