Title: Coloring Concrete-The Right Way

Author(s): William J. Mattern

Publication: Concrete International

Volume: 7

Issue: 11

Appears on pages(s): 39-41

Keywords: architectural concrete; blending; colored colors (materials); economics; iron oxides; pigments. concrete;

DOI:

Date: 11/1/1985

Abstract:
Considerations involved in selecting and using iron oxide colorants as dry additives in architectural concrete are discussed. The types of iron oxide, their differences, relative economy, effect on structural integrity, recommended loadings, and on-site blending considerations are detailed.