Title: Overview of Overlays

Author(s): Gordon K. Ray

Publication: Concrete International

Volume: 7

Issue: 10

Appears on pages(s): 23-27

Keywords: concrete pavements; reviews; structural design. performance; repairs; resurfac

DOI:

Date: 10/1/1985

Abstract:
Discusses the renewed interest in concrete resurfacing, which was probably increased by the federal funding now available for 4R projects: restoration, rehabilitation, resurfacing, and reconstruction.