Title: Icy Challenge: Concrete and Steel are Combined in arctic offshore structures

Author(s): Michael Rojansky and Yu-Yi Hsu

Publication: Concrete International

Volume: 7

Issue: 8

Appears on pages(s): 38-44

Keywords: composite construction (concrete and steel); con-fined concrete; ductility; low temperature; offshore structures; sandwich structures; structural design; walls.

DOI:

Date: 8/1/1985

Abstract:
The combined use of reinforced concrete and structural steel has produced new designs for arctic exploration and production structures. A stepped pyramid structure, using a hybrid concrete and steel material, appears to meet the stringent design requirements necessary to construct, transport, and operate such a structure.