Effects of Release Agents Used on Plywood Forms

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Release Agents Used on Plywood Forms

Author(s): Thomas Reading

Publication: Concrete International

Volume: 7

Issue: 7

Appears on pages(s): 15-22

Keywords: dusting (concrete); form removal; formwork (construction); parting agents; performance; plywood; surface defects.

DOI:

Date: 7/1/1985

Abstract:
Form release agents perform several functions in concrete construction. A large number of materials are available and there is a need for more knowledge on the properties of these materials. Several tests were conducted for evaluating the effects of release agents, and they were used to compare the performance of 30 different materials. Principal emphasis was on single-use plywood forms, but some plastic coated and paper forms were included. *