Title: Testing Early-Age Strength of Concrete In-Place

Author(s): V. M. Malhotra

Publication: Concrete International

Volume: 7

Issue: 4

Appears on pages(s): 39-41

Keywords: age-strength relation; compressive strength; concrete construction; form removal; penetration tests; pullout tests; quality control; safety.

DOI:

Date: 4/1/1985

Abstract:
Discusses the need for tests to determine the early-age strength and quality of concrete in-place. Currently available test methods and their advantages and limitations are examined. It is concluded that available in-place testing methods are adequate, although not perfect, to provide the needed information for safe form removal during construction.