Third Avenue - The First High-Rise Diagonally Braced Concrete Structure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Third Avenue - The First High-Rise Diagonally Braced Concrete Structure

Author(s): Jacob S. Grossman

Publication: Concrete International

Volume: 7

Issue: 2

Appears on pages(s): 53-56

Keywords: frames; framing systems; high-rise buildings; reinforced concrete.

DOI:

Date: 2/1/1985

Abstract: