The Aurora Australis: Design and construction of a Concrete Origami Canoe

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Aurora Australis: Design and construction of a Concrete Origami Canoe

Author(s): R. Q. Bridge and R. J. Wheen

Publication: Concrete International

Volume: 7

Issue: 1

Appears on pages(s): 31-34

Keywords: concrete construction; concrete slabs; form-work (construction); joints (junctions); reinforced con-crete; ships; structural design.

DOI:

Date: 1/1/1985

Abstract:
The concept of concrete origami has wide-ranging possibilities for the concrete industry, according to the authors. This article describes the origami concept, its refinement in two earlier canoes, and the construction of an entry for an international concrete canoe competition in Stockholm, Sweden.