Precast Concrete Bents Stacked for Style and Stability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Precast Concrete Bents Stacked for Style and Stability

Author(s): Thomas W. Kam

Publication: Concrete International

Volume: 6

Issue: 11

Appears on pages(s): 08-11

Keywords: bents; concrete construction; frames; post-tensioning; precast concrete.

DOI:

Date: 11/1/1984

Abstract:
Precast concrete bents, shaped in an inverted U, were stacked to create a frame to resist both the gravity and wind loads on the new Dallas area headquarters for Blue Cross/Blue Shield. Each bent is a monolithic concrete unit composed of two columns and one beam. The more heavily loaded bents were also post-tensioned to eliminate unsightly cracking and deflections. Use of these units reduced the number of precast ele-ments and connections for the building and served a dual role as a structural frame and architectural fea-ture.