Sulfur Concrete at AMAX Nickel -A Project Case History

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sulfur Concrete at AMAX Nickel -A Project Case History

Author(s): Scott S. Pickard

Publication: Concrete International

Volume: 6

Issue: 10

Appears on pages(s): 35-41

Keywords: acid resistance; binders (material); con-cretes; corrosion resistance; permeability; repairs; sulfur. .

DOI:

Date: 10/1/1984

Abstract:
Sulfur concrete has the potential to solve some serious industry corrosion problems. This article describes the rehabilitation of a large basement area situated beneath a copper electro-winning operation. About 29,000 ft2 (2694 m2) of deteriorated portland cement concrete floor was overlayed with 3 1/2 in. (89 mm) of unreinforced sulfur concrete. A general background of sulfur concrete, its characteristics, and a description of techniques, materials, and equipment used during construction are given. The conclusions point to the need for improvements in equipment and tech-niques to reduce costs and the need for development of standards and recommended guidelines.