301-684 Analysis of ACI Committee 350’s recommended design standards

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 301-684 Analysis of ACI Committee 350’s recommended design standards

Author(s): Anand B. Gogate

Publication: Concrete International

Volume: 6

Issue: 10

Appears on pages(s): 17-20

Keywords: concrete construction; cracking (fracturing); crack width and spacing; creep properties; economics; expansion; joint sealers; joint (junctions); safety factor; sanitary engineering; serviceability; shrinkage; struc-tural

DOI:

Date: 10/1/1984

Abstract:
The newly revised report of Committee 350, Concrete Sanitary Engineering Structures, attempts to improve a previous committee report on design, construction, and performance of such structures. This article features the changes made to the old report and notes that present design methods cannot adequately address design for creep, shrinkage, and temperature; behavior of joints; and optimum design from a cost standpoint. Serviceability, crack control, factor of safey, buildability, and economy are discussed.*