Day-to-day Comparison of 4 and 6 in. Diameter Concrete Cylinder Strengths

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Day-to-day Comparison of 4 and 6 in. Diameter Concrete Cylinder Strengths

Author(s): Chetan G. Date and Russel H. Schnormeier

Publication: Concrete International

Volume: 6

Issue: 8

Appears on pages(s): 24-26

Keywords: age-strength relation; building codes; com-pression tests; compressive strength; concretes; cylinders; evaluation; Statistical analysis.

DOI:

Date: 8/1/1984

Abstract:
At various stages of curing, strengths obtained from a 4 i n . diameter concrete cylinder are compared to those obtained from a 6 in. diameter cylinder. It was concluded that for commonly used concrete, 4-in. cylinders can be used instead of 6-in. cylinders because the difference in their strengths at any state of curing is insignificant.