Flexural Rigidity of Reinforced Concrete Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Rigidity of Reinforced Concrete Members

Author(s): Lian Duan, Fu-Ming Wang, and Wai-Fah Chen

Publication: Structural Journal

Volume: 86

Issue: 4

Appears on pages(s): 419-427

Keywords: beams (supports); deflection; flexural strength; moment-curvature relationship; reinforced concrete; stiffness; structural design.

DOI: 10.14359/9228

Date: 7/1/1989

Abstract:
A practical method for calculating the flexural rigidity of reinforced concrete members under short-time loading is proposed. This method has been developed and refined to achieve both simplicity in use and a representation of actual behavior that is as realistic as possible. Extensive comparisons of the calculated deflections have been made with the results of 434 tests of actual beams, providing final confirmation of the validity of the proposed method.