Computers Handle Quality Control

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Computers Handle Quality Control

Author(s): David F. Anderson

Publication: Concrete International

Volume: 6

Issue: 3

Appears on pages(s): 39-43

Keywords: compressive strength; computer programs; concretes; mix proportioning; optimization; quality con-trol; regression analysis; standard deviation; statistical analysis; water-cement ratio.

DOI:

Date: 3/1/1984

Abstract:
Modern statistical techniques are particularly valuable in the concrete quality control system because of the many variables involved and the repetitive individual batch method of concrete production, The twin advantages of greater economy and improved structural integrity offer a substantial benefit to the user of such methods. Widespread availability of small computers makes these controls even more attractive. Specific applications include statistical routines for measures of central tendency, measures of variability, and linear regression analysis applied to water-cement/strength ratios and prediction of future strengths.