Global Prospects for Concrete Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Global Prospects for Concrete Construction

Author(s): Fred Moavenzadeh

Publication: Concrete International

Volume: 6

Issue: 2

Appears on pages(s): 24-35

Keywords: cements; concrete construction; costs; economics; manufacturing; predictions; production methods; statistics.

DOI:

Date: 2/1/1984

Abstract:
Construction plays a vital role in the socio-economic growth of any nation, and building materials are its most important resources. Both the consumption and production of cement have been growing rapidly in the developing world and it appears that the demand for concrete in the third world may continue to escalate. The author takes a look at current trends, predicts that the use of construction materials such as concrete will rise, and urges more intense research and development.