Title: Architectural Cast-in-Place Concrete

Author(s): R. Kenney

Publication: Concrete International

Volume: 6

Issue: 1

Appears on pages(s): 50-55

Keywords: abrasive blasting; aggregates; architectural concrete; consolidation; cracking (fracturing); curing; drying shrinkage; formwork (construction); mix propor-tioning; patching; plasticizers; quality control; repairs;

DOI:

Date: 1/1/1984

Abstract:
A look at some of the things that can happen when working with architectural concrete, and their causes.