The Twentieth Century Stone

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Twentieth Century Stone

Author(s): Teodoro Gonzales De Leon

Publication: Concrete International

Volume: 6

Issue: 1

Appears on pages(s): 21-31

Keywords: architectural concrete; architecture; buildings; history; reinforced concrete.

DOI:

Date: 1/1/1984

Abstract:
Through a series of comments about important architectural works and some of the more renowned architects, the author presents a panoramic exposition of some of the different historical stages in concrete construction, including personal viewpoints and con-tributions