Title: Combined Bending and Torsion in reinforced Concrete Beams With Rectangular openings

Author(s): M. A. Mansur

Publication: Concrete International

Volume: 5

Issue: 11

Appears on pages(s): 51-58

Keywords: beams (supports); bending; frames; limit de-sign method; openings; reinforced concrete; statically indeterminate structures; structural design; tests; tor-sion.

DOI:

Date: 11/1/1983

Abstract:
Presents a simple method for the design of rein-forced concrete beams that contain a large rectangular opening and are subjected to combined bend-ing and torsion. The method is based on the concept of limit design in which torsional moments carried by the members above and below the-opening are as-




  