Recommendations for Concrete Members Prestressed With Unbonded Ten-dons

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommendations for Concrete Members Prestressed With Unbonded Ten-dons

Author(s): ACI-ASCE Committee 423

Publication: Concrete International

Volume: 5

Issue: 7

Appears on pages(s): 61-76

Keywords: anchorage (structural); beams (supports); bond (concrete to reinforcement); concrete construction; concrete slabs; corrosion; cover; cracking (fracturing); earthquake resistant structures; fire resistance; flat concrete plates; fiat concrete slabs;

DOI:

Date: 7/1/1983

Abstract:
Presented as a guide for the design of flexural structural members in buildings with unbonded tendons. Suggestions are made for needed revisions and additions to the ACI Building Code regarding this subject. Consideration is given to determining fire endurance, design for seismic forces and catastrophic loadings, and design for gravity and lateral loads. Recommendations are given concerning details and properties of tendons, protection against corrosion, and construction procedures. .