Simple Device for Carrying 6 x 12 in. Concrete Test Cylinders

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Simple Device for Carrying 6 x 12 in. Concrete Test Cylinders

Author(s): L. B. Shotwell

Publication: Concrete International

Volume: 5

Issue: 3

Appears on pages(s): 39-40

Keywords: concretes; conveying; cylinders; safety.

DOI:

Date: 3/1/1983

Abstract:
Transport of 6 x 12 in. (15.2 x 30.5 mm) concrete test cylinders is difficult at many construction sites because of the bulky nature of the test specimens. It is generally not practical to safely carry more than one test specimen at a time. A simple collapsible handle for carrying such cylinders is described.*