Title: Column Analysis With a Programmable Calculator

Author(s): Charles I. Dinsmore

Publication: Concrete International

Volume: 4

Issue: 11

Appears on pages(s): 32-36

Keywords: biaxial loads; columns; computer programs; strength; structural analysis; structural design; ultimate strength method.

DOI:

Date: 11/1/1982

Abstract:
Using the programmable calculator, a structural engineer can analyze a rectangular or circular concrete column subjected to uniaxial and biaxial bend-ing. By stress-strain compatility and the criteria established by ACI 318-77, the ultimate capacity of a column can be obtained for a specific design condition in a matter of minutes.