Properties of Dry-Mix Shotcrete Containing Supplementary Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Dry-Mix Shotcrete Containing Supplementary Cementitious Materials

Author(s): Michel Pigeon, Pierre Lacombe, Denis Bequpr , ric Cloutier

Publication: Concrete International

Volume: 22

Issue: 10

Appears on pages(s): 51-57

Keywords:

DOI:

Date: 10/1/2000

Abstract:
This article presents the results of a research project aimed at identifying mineral admixtures for potential replacement of silica fume in dry-mix shotcrete. The results showed that Type C fly ash gave the best results in terms of shotcrete properties. Length-change measurements indicated shrinkage can be significantly reduced when fly ash is used. Good compressive strengths and low absorption were obtained with the fly-ash mixtures.