Title: Photoengraving on Concrete

Author(s): Phillippe Donnaes

Publication: Concrete International

Volume: 22

Issue: 10

Appears on pages(s): 30-31

Keywords:

DOI:

Date: 10/1/2000

Abstract:
This article describes the process of photengraving on concrete by combining silk-screen printing with concrete chemistry. Examples of structures using this technique are given.