Title: Quality Assurance for Concrete Platforms in North Sea Oil Fields

Author(s): Jan Moksnes

Publication: Concrete International

Volume: 4

Issue: 9

Appears on pages(s): 13-19

Keywords: concrete construction; offshore structures: quality control.

DOI:

Date: 9/1/1982

Abstract:
Since 1971, 15 concrete gravity platforms have been built for the North Sea oil fields. These very large structures are designed and built according to rig-