Title: Guidance in the Establishment of an Inspection Program

Author(s): Claude E. Jaycox

Publication: Concrete International

Volume: 4

Issue: 9

Appears on pages(s): 79-83

Keywords: concrete construction; inspection; quality control; specifications; tests.

DOI:

Date: 9/1/1982

Abstract:
How do we successfully implement the inspection and testing requirements of the specifications? It is not enough to just reference them; we must set up a coherent written program for the guidance of inspectors. Several ways to do this are described.*