Guidance in the Training and Qualification of Inspection Personnel

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guidance in the Training and Qualification of Inspection Personnel

Author(s): Donald E. Dixon

Publication: Concrete International

Volume: 4

Issue: 9

Appears on pages(s): 84-87

Keywords: concretes; criteria; inspection; sampling; tests; training courses.

DOI:

Date: 9/1/1982

Abstract:
Programs for the training and qualification of personnel involved in sampling, testing, and inspection during construction can help assure quality con-creting. Lack of proper testing, inaccurate test data, and use of untrained personnel testing can lead to