Guide to Certification of Shotcrete Nozzlemen

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guide to Certification of Shotcrete Nozzlemen

Author(s): ACI Committee 506

Publication: Concrete International

Volume: 4

Issue: 10

Appears on pages(s): 69-71

Keywords: certification; evaluation; examinations; placing; refractory concretes; shotcrete; tanks (con-tainers); training courses.

DOI:

Date: 10/1/1982

Abstract:
This guide presents means of certifying wet and dry mix shotcrete nozzlemen for application of several, but not all, types of shotcrete. Certification procedure includes a learning and training period, a written/oral examination, and a workmanship demonstration.*