Seismic Behavior of Steel-Fiber Reinforced Concrete Interior Beam-Column Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Behavior of Steel-Fiber Reinforced Concrete Interior Beam-Column Joints

Author(s): Andre Filiatrault, Sylvain Pineau, and Jules Houde

Publication: Structural Journal

Volume: 92

Issue: 5

Appears on pages(s): 543-552

Keywords: beam-column frame; concretes; cyclic loads; ductility; earthquakes; fiber reinforced concrete fibers; joints (junctions); seismic analysis; Structural Research

DOI: 10.14359/905

Date: 11/1/1995

Abstract:
The use of steel-fiber reinforced concrete to improve the behavior of beam-column joints during earthquake excitation is investigated. Results of quasi-static tests on three full-scale interior beam-column joints and part of a prototype building designed according to the National Building Code of Canada are presented. The first specimen was made of normal concrete but ignored the special seismic recommendations related to the spacing of lateral reinforcement in the beams, column, and joint. The second specimen was also made of normal concrete and included full seismic details. The third specimen was similar to the first one but incorporated hook-end steel fibers in the joint region. Experimental results indicated that steel fibers bridging across cracks in the concrete mix increase the joint shear strength and can diminish requirements for closely spaced ties.