Abstract:
This summary article condenses a detailed report which describes 112 fibrous concrete projects and applications throughout the world. It includes descrip-tions of construction procedures, mix proportions, and properties for both steel fibrous concrete and glass fiber reinforced concrete. Typical applications include structures, airfield and highway overlays, shotcrete applications, and other uses.