Should I Promote Concrete?

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Should I Promote Concrete?

Author(s): Maurice L. Burgener

Publication: Concrete International

Volume: 2

Issue: 11

Appears on pages(s): 30-33

Keywords: concrete construction; concrete durability; concrete products; economics; structural design.

DOI:

Date: 11/1/1980

Abstract:
The case histories outlined in this article show how various individuals and groups influence the total use of concrete at the same time they promote their own services. The fact that individuals of many diverse interests join ACI indicates their widespread interest in concrete. If all these diverse interests concentrated on promoting more concrete construction, concrete would easily achieve an overwhelming predominance as a construction material. [Author]