Guide for Repair of Concrete Bridge Superstructures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guide for Repair of Concrete Bridge Superstructures

Author(s): ACI Committee 546

Publication: Concrete International

Volume: 2

Issue: 9

Appears on pages(s): 69-88

Keywords: bridges (structures); concretes; concrete. construction; epoxy resins; latex (plastic); plastics, polymers, and resins; repairs; shotcrete.

DOI:

Date: 6/1/1980

Abstract:
Repair techniques for concrete bridge superstructures are described. This includes pier caps, beams, decks, curbs, sidewalks, and rails. Special emphasis is placed on decks. Recommendations for evaluation of damage, selection of repair method, and surface preparation are given. Repair materials given primary consideration are conventional portland cement mor-tars and concretes and those using latex, epoxy resins, or methyl methacrylate. Other techniques that have been documented and used extensively are included. Guide recommendations are those considered necessary for severe exposure conditions. .