Title: Implace Loads and Tiltmup Bearing Walls -A Design Approach

Author(s): K. M. Kripanarayanan

Publication: Concrete International

Volume: 2

Issue: 4

Appears on pages(s): 43-47

Keywords: bearing walls; concrete panels; loads (forces); moments; precast concrete; reinforcing steels; slenderness ratio; structural analysis; tilt-up construction.

DOI:

Date: 4/1/1980

Abstract:
The PCA design aid method to analyze load-bearing -tilt- up walls for in-place loads is presented. This method is within the scope of Building Code Re-quirements for Reinforced Concrete (AC1 318077). Also, it takes into account factors such as slenderness ratios, reinforcement ratios, and secondary moments. [Author]