Survey of Parking Structure Deterioration and Distress

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Survey of Parking Structure Deterioration and Distress

Author(s): Carl A. Peterson

Publication: Concrete International

Volume: 2

Issue: 3

Appears on pages(s): 53-61

Keywords: concrete slabs; corrosion; cracking (frac-turing); deicers; deterioration; freeze-thaw durability; garages; parking facilities; reinforcing steels; scaling.

DOI:

Date: 3/1/1980

Abstract:
Parking structures in the United States are subjected to different thermal, moisture, and chemical environments. This article primarily deals with ob-served deterioration and distress of open, unheated parking structures located in climates where deicing salts are used on nearby roads and highways. Some of the observations made, however, may apply to other structures and exposures. [Author]